General
Property | Temperature | Value | |
---|---|---|---|
Calibrado | 23.0 °C | 1.3 % Show Material materials with Calibrado of 1.3 % | |
Densidad | 23.0 °C | 1.76 g/cm³ Show Material materials with Densidad of 1.76 g/cm³ | |
Densidad lineal | 23.0 °C | 4.00E+7 g/cm Show Material materials with Densidad lineal of 4.00E+7 g/cm | |
Número de filamentos | 23.0 °C | 6000 [-] Show Material materials with Número de filamentos of 6000 [-] | |
Tex | 23.0 °C | 400 [-] Show Material materials with Tex of 400 [-] | |
Tipo de fibra | PAN carbon fiber |
Medidas
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] |
Elongación | 23.0 °C | 1.7 % Show Material materials with Elongación of 1.7 % |
Módulo elástico | 23.0 °C | 238 GPa Show Material materials with Módulo elástico of 238 GPa |
Resistencia a la tracción | 23.0 °C | 3950 MPa Show Material materials with Resistencia a la tracción of 3950 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 710 J/(kg·K) Show Material materials with Calor específico of 710 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | -1E-7 1/K Show Material materials with Coeficiente de dilatación térmica of -1E-7 1/K |
Conductividad térmica | 23.0 °C | 17 W/(m·K) Show Material materials with Conductividad térmica of 17 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 1.6E-5 Ω·m Show Material materials with Resistividad eléctrica of 1.6E-5 Ω·m |
Technological properties
Property | ||
---|---|---|
Processing history | Epoxy sized 1.2% |