General
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de permeabilidad | 23.0 °C | 2E-5 cm²/s Show Material materials with Coeficiente de permeabilidad of 2E-5 cm²/s | for air through plane |
Densidad aparente | 23.0 °C | 1 g/cm³ Show Material materials with Densidad aparente of 1 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 30 [-] Show Material materials with Dureza Shore D of 30 [-] | |
Elongación | 23.0 °C | 1 % Show Material materials with Elongación of 1 % | |
Factor de compresibilidad | 23.0 °C | 45 % Show Material materials with Factor de compresibilidad of 45 % | DIN 28090-2 |
Factor de compresión de fluencia en caliente | 23.0 °C | 3 % Show Material materials with Factor de compresión de fluencia en caliente of 3 % | DIN 28090-2 |
Factor de junta "m" | 23.0 °C | 2 N/mm² Show Material materials with Factor de junta "m" of 2 N/mm² | |
Factor de junta "y" | 23.0 °C | 10 N/mm² Show Material materials with Factor de junta "y" of 10 N/mm² | |
Factor de recuperación de compresión | 20.0 °C | 5 % Show Material materials with Factor de recuperación de compresión of 5 % | DIN 28090-2 |
300.0 °C | 4 % Show Material materials with Factor de recuperación de compresión of 4 % | DIN 28090-2 | |
Módulo elástico | 23.0 °C | 0.7 GPa Show Material materials with Módulo elástico of 0.7 GPa | DIN 28090-1 |
Resistencia a la tracción | 23.0 °C | 4 MPa Show Material materials with Resistencia a la tracción of 4 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 1000.0 °C | 1E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-6 1/K | |
Coeficiente de dilatación térmica transversal | 1000.0 °C | 5E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 5E-5 1/K | |
Conductividad térmica | 20.0 °C | 200 W/(m·K) Show Material materials with Conductividad térmica of 200 W/(m·K) | |
Contenido de cenizas | 23.0 °C | 0.15 % Show Material materials with Contenido de cenizas of 0.15 % | DIN 51903 |
Thermal conductivity, through-plane | 20.0 °C | 5 W/(m·K) Show Material materials with Thermal conductivity, through-plane of 5 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 8E-6 Ω·m Show Material materials with Resistividad eléctrica of 8E-6 Ω·m |
Resistividad eléctrica transversal | 20.0 °C | 6.5E-4 Ω·m Show Material materials with Resistividad eléctrica transversal of 6.5E-4 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | |
Carbono | 99.85 % Show Material materials with Carbono of 99.85 % | |
Cloro | 1E-3 % Show Material materials with Cloro of 1E-3 % | |
Flúor | 1E-3 % Show Material materials with Flúor of 1E-3 % | |
Otro | 5E-3 % Show Material materials with Otro of 5E-3 % | halogen content |
Technological properties
Property | ||
---|---|---|
Application areas | Metallic gaskets such as spiral wound gaskets, corrugated metal gaskets and kammprofile gaskets, compression packing for stuffing boxes | |
Corrosion inhibitor | Passive corrosion inhibitor (ASTM F 2168-13) | |
Other | The key feautres are: Soft and flexible, inert and highly impermeable to gases and liquids, fire safe; Asbestos-free, no associated health risks; Free of any polymers or organic binders; No aging or fatigue under dynamic load even at elevated temperatures; Even in long term services, no noticeable changes in properties; No measurable cold or warm flow characteristics up to the maximum permissible gasket stress; Electrically conductive, no static charge; Excellent chemical resistance and high thermal shock capability; Operating temperatures from cryogenic to super-heated steam temperature. Life time might be limited by the joint design, actual equipment temperatures and operating temperatures; Easy handling and processability during assembly or punching | |
Oxidation inhibitor | Yes |