General
Property | Value |
---|---|
Tamaño del dominio | 10 - 20 μm Show Material materials with Tamaño del dominio of 10 - 20 μm |
Sustrato | PET, 188µm |
Medidas
Eléctrico
Property | Temperature | Value |
---|---|---|
Movilidad de los portadores | 23.0 °C | 3500 cm²/Vs Show Material materials with Movilidad de los portadores of 3500 cm²/Vs |
Surface resistivity | 23.0 °C | 250 - 400 Ω/sq Show Material materials with Surface resistivity of 250 - 400 Ω/sq |
Óptico
Property | Value |
---|---|
Transmisión lumínica | 97 [-] Show Material materials with Transmisión lumínica of 97 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Light flexible displays, plastic electronics, printed circuit boards, liquid crystal displays, thin film photovoltaics, e-paper, sensors and OLEDs | |
Processing history | Growth method: CVD |