General
Property | Value |
---|---|
Tamaño de grano | 20 μm Show Material materials with Tamaño de grano of 20 μm |
Medidas
Property | Value | Comment |
---|---|---|
Espesor | 3.45E-7 mm Show Material materials with Espesor of 3.45E-7 mm | theoretical thickness of graphene monolayer |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Movilidad de los portadores | 23.0 °C | 3760 cm²/Vs Show Material materials with Movilidad de los portadores of 3760 cm²/Vs | FET Electron Mobility on SiO₂/Si substrate |
Surface resistivity | 23.0 °C | 410 - 490 Ω/sq Show Material materials with Surface resistivity of 410 - 490 Ω/sq | Van der Pauw sheet resistance on SiO₂/Si substrate (1cm x 1cm) |
Óptico
Property | Value |
---|---|
Transmisión lumínica | 97 [-] Show Material materials with Transmisión lumínica of 97 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Graphene research, flexible batteries, electronics, aerospace industry, MEMS and NEMS, microactuators, conductive coatings | |
Other | "Easy Transfer": avoids metal etching, avoids hazardous chemical handling, bottom layer removed. Coverage of >98%. | |
Processing history | Growth method: CVD. Processed in Clean Room Class 1000. |