Mica has an estimable electrical, physical, mechanical and thermal pertinacity properties. It has high transparency, optical clarity, flatness, non-breakability and heat resistance. As such, it is suitably used as windows in Kerosene stove, Wood stoves, Furnace peep-holes and microwave ovens.


Mica eliminates risk of cracks, breakage, jerks and can easily withstand shocks, strains and vibration during operations at higher temperatures and prevent grassing. Mica also provide complete safety, versatility, durability and reliability and retain its basic strength.


Mica sheet can be expose to high temperature up to ~ 540 °C (~1000F)

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

General

PropertyTemperatureValue

Densidad

23.0 °C

2.6 - 3.2 g/cm³

Show Material materials with Densidad of 2.6 - 3.2 g/cm³

Mecánica

PropertyTemperatureValue

Dureza (en mohs)

23.0 °C

2 - 3.2 [-]

Show Material materials with Dureza (en mohs) of 2 - 3.2 [-]

Resistencia a la tracción

23.0 °C

255 - 296 MPa

Show Material materials with Resistencia a la tracción of 255 - 296 MPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

25.0 °C

0.21 J/(kg·K)

Show Material materials with Calor específico of 0.21 J/(kg·K)

Coeficiente de dilatación térmica

200.0 °C

8E-6 - 9E-6 1/K

Show Material materials with Coeficiente de dilatación térmica of 8E-6 - 9E-6 1/K

500.0 °C

1E-5 - 1.2E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.2E-5 1/K

Coeficiente de dilatación térmica transversal

100.0 °C

1.5E-5 - 2.5E-5 1/K

Show Material materials with Coeficiente de dilatación térmica transversal of 1.5E-5 - 2.5E-5 1/K

300.0 °C

1.5E-5 - 2.5E-5 1/K

Show Material materials with Coeficiente de dilatación térmica transversal of 1.5E-5 - 2.5E-5 1/K

600.0 °C

1.6E-5 - 3.6E-5 1/K

Show Material materials with Coeficiente de dilatación térmica transversal of 1.6E-5 - 3.6E-5 1/K

Unlock all property charts

Conductividad térmica

23.0 °C

8 W/(m·K)

Show Material materials with Conductividad térmica of 8 W/(m·K)

Temperatura máx. de funcionamiento

400 - 500 °C

Show Material materials with Temperatura máx. de funcionamiento of 400 - 500 °C

no decomposition

Eléctrico

PropertyTemperatureValueComment

Constante dieléctrica

23.0 °C

6.5 - 9 [-]

Show Material materials with Constante dieléctrica of 6.5 - 9 [-]

Factor de potencia

25.0 °C

0.08 - 0.09 [-]

Show Material materials with Factor de potencia of 0.08 - 0.09 [-]

60 cycles

Resistividad eléctrica

23.0 °C

1.00E+10 - 1.00E+13 Ω·m

Show Material materials with Resistividad eléctrica of 1.00E+10 - 1.00E+13 Ω·m

Óptico

PropertyValue

Ángulo óptico axial

38 - 47 °

Show Material materials with Ángulo óptico axial of 38 - 47 °

Índice de refracción, α

1.55 - 1.57 [-]

Show Material materials with Índice de refracción, α of 1.55 - 1.57 [-]

Índice de refracción, β

1.58 - 1.61 [-]

Show Material materials with Índice de refracción, β of 1.58 - 1.61 [-]

Índice de refracción, γ

1.59 - 1.61 [-]

Show Material materials with Índice de refracción, γ of 1.59 - 1.61 [-]

Orientación del plano óptico

Perpendicular to plane of symmetry

Technological properties

Property
Application areas

Rigid or flexible mica sheets can be used for electrical insulating, high temperature mica washers, mica gaskets, heaters manufacturing and many other applications