Mecánica
Property | Temperature | Value |
---|---|---|
Resistencia a la tracción | 23.0 °C | 0.15 MPa Show Material materials with Resistencia a la tracción of 0.15 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Conductividad térmica | 1000.0 °C | 0.4 W/(m·K) Show Material materials with Conductividad térmica of 0.4 W/(m·K) | |
Temperatura máx. de funcionamiento | 3000 °C Show Material materials with Temperatura máx. de funcionamiento of 3000 °C | in vacuum | |
Temperatura máx. de funcionamiento, inerte | 3600 °C Show Material materials with Temperatura máx. de funcionamiento, inerte of 3600 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 1.4E-3 Ω·m Show Material materials with Resistividad eléctrica of 1.4E-3 Ω·m |
Chemical properties
Property | Value |
---|---|
Carbono | 99.96 % Show Material materials with Carbono of 99.96 % |
Technological properties
Property | ||
---|---|---|
Application areas | Vacuum and High Pressure Sintering Industry: Heat Insulation for Metal Sintering, Non Oxide Ceramics, Tungsten Carbide manufacturing; Vacuum Treatment Industry: Heat Insulation for Commercial Heat Treat Furnaces, Hardening, Tempering, etc. Crystal Growing Industry: Heat Insulation for silicon, Sic, Indium phosphide, Gallium Arsenide, Sapphire, Optical Crystals, Solar Ingots; Special Casting Industry: Heat Insulation for precision casting of DS/SC turbine engine components and Metal Matrix Composites.Graphitizing/CVD Applications: Heat Insulation for High Modulus Carbon Fiber Production, Halogen purification Furnaces; Electronic/Semiconductor Industry: Heat Insulation for Materials for various precursor applications; Aerospace Industry: Hot isostatic process furnaces, heat treating, sintering, brazing furnaces, autoclaves; Solar cells: graphite felt electrode in the vanadium redox flow battery. Filtering materials of scorching gas, liquid and fused metal; Perforated electrode of fuel battery, Catalyst carrier; Face of corrosion resistant materials; Semi-Conductor: as insulation boards and cylinders using together with high purified graphite crucibles, heating elements and other elements within the hot zone; As the raw materials for producing Rigid Felt boards; The 2.5 mm - 3 mm thick rayon graphite felt to be cut into strips as the light and heat filament in “BATHROOMMASTER” and “Quartz tube heating lamp”; Furnace - resistance or induction heated vacuum furnaces and inert gas furnaces, such as degassing furnaces, brazing furnaces, soft and bright annealing furnaces, sintering furnaces for hard metals, carburizing furnaces, laboratory graphitizing furnaces; inductively heated melting and heat treatment furnaces, in which a proportion of the ceramic insulating material is replaced by felt in order to increase the electrical efficiency and prevent the liquid metal from coming into contact with the induction coil in the event of crucible fracture (no wetting); Thermal insulation, as filters, and as catalyst support; Porous electrodes and Turbine blade manufacturing |