Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Multi Wall Carbon Nanotubes “Chunky” Powder NC006060 (>90% purity)
Free Standing aligned CNT arrays (Carpets) are synthesized by floating catalyst CVD method within a horizontal quartz reaction tube.
The CNT synthesis parameters are carefully selected to provide maximum-yield of CNT growth, high packing density as well as high graphitization level.
Los datos sobre este material han sido proporcionados por Matmatch.
All categories
Let us help you find the best supplier!
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationGeneral
Property | Value |
---|---|
Nivel de grafitización | 0.3 - 0.4 [-] Show Material materials with Nivel de grafitización of 0.3 - 0.4 [-] |
Medidas
Property | Value |
---|---|
Diámetro de nanotubos | 30 - 90 nm Show Material materials with Diámetro de nanotubos of 30 - 90 nm |
Longitud del nanotubo | 300 - 1000 µm Show Material materials with Longitud del nanotubo of 300 - 1000 µm |
Aplicaciones térmicas
Property | Value |
---|---|
Límite de oxidación | 600 - 700 °C Show Material materials with Límite de oxidación of 600 - 700 °C |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.