Epoxy Resin ТO200

Want to keep this datasheet? Save it now in your required format

Description

ТО200 is a two-part epoxy resin with unique characteristics, combining high heat resistance, strength and processability. The impregnation temperature is 20-25°C. Flexible curing mode in combination with post-curing allows achieving the required heat resistance at the minimum curing temperature. It shows the following features and properties:


  • Wide processing window >2 hours at 25°C
  • Curing at room temperature
  • Tracking of infusion process under UV light
  • Low exotherm
  • High mechanical properties
  • For tooling up to 200°C
  • Los datos sobre este material han sido proporcionados por Matmatch.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Propiedades

    General

    PropertyTemperatureValueComment

    Densidad

    23.0 °C

    1.15 g/cm³

    Show Material materials with Densidad of 1.15 g/cm³

    ASTM D792

    Mecánica

    PropertyTemperatureValueComment

    Módulo elástico

    23.0 °C

    3.26 GPa

    Show Material materials with Módulo elástico of 3.26 GPa

    ASTM D638

    Plane-Strain Fracture Toughnes

    23.0 °C

    0.64 MPa·√m

    Show Material materials with Plane-Strain Fracture Toughnes of 0.64 MPa·√m

    ASTM D5045

    Resistencia a la flexión

    23.0 °C

    94 MPa

    Show Material materials with Resistencia a la flexión of 94 MPa

    ASTM D790

    Resistencia a la tracción

    23.0 °C

    60 MPa

    Show Material materials with Resistencia a la tracción of 60 MPa

    ASTM D638

    Liberación de energía de deformación

    ASTM D5045

    Aplicaciones térmicas

    PropertyTemperatureValueComment

    Coeficiente de dilatación térmica

    23.0 °C

    8.7E-5 1/K

    Show Material materials with Coeficiente de dilatación térmica of 8.7E-5 1/K

    ASTM E831

    Temperatura de impregnación

    20 - 25 °C

    Show Material materials with Temperatura de impregnación of 20 - 25 °C

    Temperatura de transición del vidrio

    211 °C

    Show Material materials with Temperatura de transición del vidrio of 211 °C

    ASTM E2092

    Temperatura máx. de funcionamiento

    120 - 180 °C

    Show Material materials with Temperatura máx. de funcionamiento of 120 - 180 °C

    for manufacturing CFRP and GFRP or for composite tooling respectively.

    Technological properties

    Property
    Application areas

    The resin can be used for manufacturing CFRP or GFRP with sustainable properties up to 120°C, or for composite tooling with service temperatures up to 180°C.

    Processing methods

    Thoroughly mix components A and B at 25°C in a 1:0.4388 weight ratio. It is recommended to use device with automatic mixing and mix under vacuum. Degas the resin with intensive mixing for 15-30 minutes at 20-25°С, pressure no more than 10 mbar. Assemble vacuum bag. Perform a leak test, the rate of the vacuum loss should not be more than 1 mbar per minute. The residual pressure in the bag must not be more than 10 mbar. Assemble the second vacuum bag. Carry out a leak test of the second vacuum bag with same conditions. The recommended impregnation temperature is 25°C. It is recommended to preliminarily dry the reinforcing material in a vacuum bag at 60-80°C for at least 1 h or 6 h at 25°C. Maintaining the temperature of the mold at 20-30°C, start the infusion process. After complete impregnation, close the resin inputs, continue evacuation from inner bag for at least 30 minutes at 25-40°C. Close the outputs from the inner bag. Continue evacuation from outer vacuum bag until gelation (~24 h at 25°C). After 48-72 hours, you can remove the part from the mold and post-cure. Post-cure: Increase the temperature at a rate of 5°C/h to 80°C then at rate 10-15°C/h to 180°C, dwell for 1 hour (or with step mode same as in picture). Highest mechanical properties of CFRP are achieved at a temperature of 80-120°C. When cured at higher temperatures, a higher heat resistance is achieved with a slight fall in the mechanical characteristics of the CFRP.