General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 150 - 190 [-] Show Material materials with Dureza Vickers of 150 - 190 [-] | |
Elongación A50 | 23.0 °C | 8 % Show Material materials with Elongación A50 of 8 % | |
Límite elástico Rp 0,2 | 23.0 °C | 450 MPa Show Material materials with Límite elástico Rp 0,2 of 450 MPa | |
Módulo elástico | 23.0 °C | 137 GPa Show Material materials with Módulo elástico of 137 GPa | cold formed |
Plegabilidad 180 ° bidireccional | 23.0 °C | 2 [-] Show Material materials with Plegabilidad 180 ° bidireccional of 2 [-] | r = x t, t <0.5mm |
Plegabilidad 180 ° en peso bruto | 23.0 °C | 2 [-] Show Material materials with Plegabilidad 180 ° en peso bruto of 2 [-] | r = x t, t <0.5mm |
Plegabilidad 90 ° bidireccional | 23.0 °C | 1.5 [-] Show Material materials with Plegabilidad 90 ° bidireccional of 1.5 [-] | r = x t, t <0.5mm |
Plegabilidad 90 ° en peso bruto | 23.0 °C | 1.5 [-] Show Material materials with Plegabilidad 90 ° en peso bruto of 1.5 [-] | r = x t, t <0.5mm |
Resistencia a la tracción | 23.0 °C | 480 - 560 MPa Show Material materials with Resistencia a la tracción of 480 - 560 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 381 J/(kg·K) Show Material materials with Calor específico of 381 J/(kg·K) | |
Coeficiente de dilatación térmica | 300.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | for 20°C to the mentioned temperature |
Conductividad térmica | 23.0 °C | 330 W/(m·K) Show Material materials with Conductividad térmica of 330 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.00E+7 - 5.30E+7 S/m Show Material materials with Conductividad eléctrica of 5.00E+7 - 5.30E+7 S/m |
Specific Electrical conductivity | 86 % IACS Show Material materials with Specific Electrical conductivity of 86 % IACS |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Circonio | 0.05 - 0.25 % Show Material materials with Circonio of 0.05 - 0.25 % | ||
Cobre | Balance | ||
Cromo | 0.2 - 1.2 % Show Material materials with Cromo of 0.2 - 1.2 % | ||
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % | max. | |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive: Switches and Relays, Contacts, Connectors, Terminals, Press fits, Hybrid Cars. Electrical: Switches and Relays, Contacts, Connectors, Terminals, Press fits, Components for the electrical industry, Stamped parts, Semiconductor Components, Junction Boxes, Photovoltaic Systems. | |
Brazing | Excellent | |
Cold Forming | Good | |
Corrosion properties | STOL® 95 is resistant to pure water vapour and non oxidizingacids and alkalis as well as neutral saline solutions. The material is insensitive to stress corrosion cracking. | |
Heat Treatment | Temper: R480 | |
Machining | Rating 20, less suitable | |
Other | This alloy is in accordance with RoHS 2002/96/CE for electric & electronic equipments and 2002/53/CE for automotive industry. It is suitable for high voltage applications as hybrid cars or photovoltaics. | |
Plating | Electroplating is excellent | |
Welding | Gas Shielded Arc Welding: Excellent, Laser Welding: Fair |