General
Property | Temperature | Value | |
---|---|---|---|
Densidad | 23.0 °C | 7.65 g/cm³ Show Material materials with Densidad of 7.65 g/cm³ | |
Estructura de grano | Grain oriented electrical steel |
Medidas
Property | Value |
---|---|
Espesor | 0.3 mm Show Material materials with Espesor of 0.3 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell B | 23.0 °C | 75 - 85 [-] Show Material materials with Dureza Rockwell B of 75 - 85 [-] | 15T |
Dureza Vickers 0,1 | 23.0 °C | 175 - 195 [-] Show Material materials with Dureza Vickers 0,1 of 175 - 195 [-] | |
Elongación A80 | 23.0 °C | 6 - 14 % Show Material materials with Elongación A80 of 6 - 14 % | |
Elongación A80 transversal | 23.0 °C | 24 - 48 % Show Material materials with Elongación A80 transversal of 24 - 48 % | |
Límite elástico Rp 0,2 | 23.0 °C | 300 - 340 MPa Show Material materials with Límite elástico Rp 0,2 of 300 - 340 MPa | |
Límite elástico transversal Rp 0,2 | 23.0 °C | 330 - 360 MPa Show Material materials with Límite elástico transversal Rp 0,2 of 330 - 360 MPa | |
Resistencia a la tracción | 23.0 °C | 330 - 370 MPa Show Material materials with Resistencia a la tracción of 330 - 370 MPa | |
Resistencia a la tracción transversal | 23.0 °C | 390 - 420 MPa Show Material materials with Resistencia a la tracción transversal of 390 - 420 MPa |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura máx. de funcionamiento | 840 °C Show Material materials with Temperatura máx. de funcionamiento of 840 °C | according to DIN IEC 60404-12, under inert gas for 2 h |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistencia al aislamiento superficial | 23.0 °C | 10 Ω·cm² Show Material materials with Resistencia al aislamiento superficial of 10 Ω·cm² | according to DIN IEC 60404-11 |
Resistividad eléctrica | 23.0 °C | 4.8E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.8E-7 Ω·m |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Fuerza coercitiva | 23.0 °C | 5 A/m Show Material materials with Fuerza coercitiva of 5 A/m | |
Polarización de saturación | 23.0 °C | 2.03 T Show Material materials with Polarización de saturación of 2.03 T | |
Polarización garantizada | 23.0 °C | 1.88 [-] Show Material materials with Polarización garantizada of 1.88 [-] | at 800 A/m |
Polarización normal | 23.0 °C | 1.91 [-] Show Material materials with Polarización normal of 1.91 [-] | at 800 A/m |
Pérdida en el núcleo garantizada | 23.0 °C | 1.05 [-] Show Material materials with Pérdida en el núcleo garantizada of 1.05 [-] | at 1.7 T and 50 Hz |
Pérdida en el núcleo normal | 23.0 °C | 1.03 [-] Show Material materials with Pérdida en el núcleo normal of 1.03 [-] | at 1.7 T and 50 Hz |
Temperatura de Curie | 745 °C Show Material materials with Temperatura de Curie of 745 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Large power transformers, distribution transformers, small transformers, current transformers, shunt reactors, wound cores, power generators | |
Coating | Both sides coated, coating thickness: 2 µm - 5 µm | |
Other | Advantages of powercore®: Energy efficiency thanks to minimal losses at full load and reduced no-load losses, reduced noise emission thanks to minimized magnetostriction and improved insulation properties, cost benefits thanks to lower core weights and more compact dimensions. |