General
Property | Value | Shape |
---|---|---|
Densidad | 4.51 g/cm³ Show Material materials with Densidad of 4.51 g/cm³ | Sheet, Plate |
Medidas
Property | Value | Shape |
---|---|---|
Ancho | 400 mm Show Material materials with Ancho of 400 mm | Sheet |
600 mm Show Material materials with Ancho of 600 mm | Plate | |
1524 mm Show Material materials with Ancho of 1524 mm | Sheet | |
1600 mm Show Material materials with Ancho of 1600 mm | Plate | |
Longitud | 1500 mm Show Material materials with Longitud of 1500 mm | Sheet, Plate |
5000 mm Show Material materials with Longitud of 5000 mm | Sheet | |
6500 mm Show Material materials with Longitud of 6500 mm | Plate |
valueMetaData
Property | Value |
---|
Mecánica
Property | Value | Shape | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.361 [-] Show Material materials with Coeficiente de Poisson of 0.361 [-] | Typical for Pure Titanium | |
Dureza Brinell | 200.0 Show Material materials with Dureza Brinell of 200.0 | Sheet, Plate | |
Límite elástico | 485.0 MPa Show Material materials with Límite elástico of 485.0 MPa | Sheet, Plate | |
Módulo de cizallamiento | 46.0 GPa Show Material materials with Módulo de cizallamiento of 46.0 GPa | Typical for Pure Titanium | |
Módulo elástico | 106.0 GPa Show Material materials with Módulo elástico of 106.0 GPa | Sheet, Plate | |
Resistencia a la tracción | 550.0 MPa Show Material materials with Resistencia a la tracción of 550.0 MPa | Sheet, Plate |
Aplicaciones térmicas
Property | Value | Shape | Comment |
---|---|---|---|
Calor específico | 540 J/(kg·K) Show Material materials with Calor específico of 540 J/(kg·K) | Sheet, Plate | |
Coeficiente de dilatación térmica | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | |
Conductividad térmica | 18 W/(m·K) Show Material materials with Conductividad térmica of 18 W/(m·K) | Sheet, Plate | |
Temperatura de fusión | 1670.0 °C Show Material materials with Temperatura de fusión of 1670.0 °C | Typical for Pure Titanium |
Chemical properties
Property | Value | Shape |
---|---|---|
Carbono | 0.08 Show Material materials with Carbono of 0.08 | Sheet, Plate |
Hidrógeno | 0.015 Show Material materials with Hidrógeno of 0.015 | Sheet, Plate |
Hierro | 0.5 Show Material materials with Hierro of 0.5 | Sheet, Plate |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | Sheet, Plate |
Oxígeno | 0.4 Show Material materials with Oxígeno of 0.4 | Sheet, Plate |