General
Property | Value | Related Standards | Shape |
---|---|---|---|
Densidad | 4.5 g/cm³ Show Material materials with Densidad of 4.5 g/cm³ | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Medidas
Property | Value | Related Standards | Shape |
---|---|---|---|
Ancho | 400 mm Show Material materials with Ancho of 400 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet |
600 mm Show Material materials with Ancho of 600 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Plate | |
1524 mm Show Material materials with Ancho of 1524 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet | |
1600 mm Show Material materials with Ancho of 1600 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Plate | |
Longitud | 1500 mm Show Material materials with Longitud of 1500 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
5000 mm Show Material materials with Longitud of 5000 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet | |
6500 mm Show Material materials with Longitud of 6500 mm | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Plate |
valueMetaData
Property | Value |
---|
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.361 [-] Show Material materials with Coeficiente de Poisson of 0.361 [-] | Typical for Pure Titanium | ||
Dureza Brinell | 150.0 Show Material materials with Dureza Brinell of 150.0 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Límite elástico | 275.0 MPa Show Material materials with Límite elástico of 275.0 MPa | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Módulo de cizallamiento | 46.0 GPa Show Material materials with Módulo de cizallamiento of 46.0 GPa | Typical for Pure Titanium | ||
Módulo elástico | 108.0 GPa Show Material materials with Módulo elástico of 108.0 GPa | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Resistencia a la tracción | 345.0 MPa Show Material materials with Resistencia a la tracción of 345.0 MPa | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Aplicaciones térmicas
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Calor específico | 520 J/(kg·K) Show Material materials with Calor específico of 520 J/(kg·K) | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Coeficiente de dilatación térmica | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | ||
Conductividad térmica | 17 W/(m·K) Show Material materials with Conductividad térmica of 17 W/(m·K) | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate | |
Temperatura de fusión | 1670.0 °C Show Material materials with Temperatura de fusión of 1670.0 °C | Typical for Pure Titanium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Carbono | 0.08 Show Material materials with Carbono of 0.08 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Hidrógeno | 0.015 Show Material materials with Hidrógeno of 0.015 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Hierro | 0.3 Show Material materials with Hierro of 0.3 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Nitrógeno | 0.03 Show Material materials with Nitrógeno of 0.03 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Oxígeno | 0.25 Show Material materials with Oxígeno of 0.25 | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |
Paladio | 0.12 - 0.25 % Show Material materials with Paladio of 0.12 - 0.25 % | ASME SB-363, ASME SB-381, ASME SB-337, ASME SB-338, ASME SB-348, ASME SB-265, UNS R52400 | Sheet, Plate |