General
Property | Value | Shape |
---|---|---|
Densidad | 4.45 g/cm³ Show Material materials with Densidad of 4.45 g/cm³ | Sheet, Plate |
Medidas
Property | Value | Shape |
---|---|---|
Ancho | 400 mm Show Material materials with Ancho of 400 mm | Sheet |
600 mm Show Material materials with Ancho of 600 mm | Plate | |
1524 mm Show Material materials with Ancho of 1524 mm | Sheet | |
1600 mm Show Material materials with Ancho of 1600 mm | Plate | |
Longitud | 1500 mm Show Material materials with Longitud of 1500 mm | Sheet, Plate |
5000 mm Show Material materials with Longitud of 5000 mm | Sheet | |
6500 mm Show Material materials with Longitud of 6500 mm | Plate |
valueMetaData
Property | Value |
---|
Mecánica
Property | Value | Shape |
---|---|---|
Límite elástico | 760.0 MPa Show Material materials with Límite elástico of 760.0 MPa | Sheet, Plate |
Módulo elástico | 110.0 GPa Show Material materials with Módulo elástico of 110.0 GPa | Sheet, Plate |
Resistencia a la tracción | 825.0 - 860.0 MPa Show Material materials with Resistencia a la tracción of 825.0 - 860.0 MPa | Sheet, Plate |
Aplicaciones térmicas
Property | Value | Shape | Comment |
---|---|---|---|
Calor específico | 560 J/(kg·K) Show Material materials with Calor específico of 560 J/(kg·K) | Sheet, Plate | |
Coeficiente de dilatación térmica | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | |
Conductividad térmica | 6.9 W/(m·K) Show Material materials with Conductividad térmica of 6.9 W/(m·K) | Sheet, Plate | |
Temperatura de fusión | 1500.0 - 1750.0 °C Show Material materials with Temperatura de fusión of 1500.0 - 1750.0 °C | Typical for Titanium Alpha Beta Alloy |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminio | 5.5 - 6.5 % Show Material materials with Aluminio of 5.5 - 6.5 % | Sheet, Plate |
Carbono | 0.08 Show Material materials with Carbono of 0.08 | Sheet, Plate |
Hidrógeno | 0.015 Show Material materials with Hidrógeno of 0.015 | Sheet, Plate |
Hierro | 0.25 Show Material materials with Hierro of 0.25 | Sheet, Plate |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | Sheet, Plate |
Oxígeno | 0.13 Show Material materials with Oxígeno of 0.13 | Sheet, Plate |
Vanadio | 3.5 - 4.5 % Show Material materials with Vanadio of 3.5 - 4.5 % | Sheet, Plate |