General
Property | Value | Shape | Related Standards |
---|---|---|---|
Densidad | 4.54 g/cm³ Show Material materials with Densidad of 4.54 g/cm³ | Sheet, Plate, Billet | |
4.54 g/cm³ Show Material materials with Densidad of 4.54 g/cm³ | Billet | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 |
Medidas
Property | Value | Shape |
---|---|---|
Ancho | 400 mm Show Material materials with Ancho of 400 mm | Sheet |
600 mm Show Material materials with Ancho of 600 mm | Plate | |
1524 mm Show Material materials with Ancho of 1524 mm | Sheet | |
1600 mm Show Material materials with Ancho of 1600 mm | Plate | |
Diámetro | 130 mm Show Material materials with Diámetro of 130 mm | Billet |
350 mm Show Material materials with Diámetro of 350 mm | Billet | |
Longitud | 1500 mm Show Material materials with Longitud of 1500 mm | Sheet, Plate |
3000 mm Show Material materials with Longitud of 3000 mm | Billet | |
4500 mm Show Material materials with Longitud of 4500 mm | Billet | |
5000 mm Show Material materials with Longitud of 5000 mm | Sheet | |
6500 mm Show Material materials with Longitud of 6500 mm | Plate |
valueMetaData
Property | Value |
---|
Mecánica
Property | Value | Shape | Related Standards |
---|---|---|---|
Coeficiente de Poisson | 0.32 [-] Show Material materials with Coeficiente de Poisson of 0.32 [-] | Sheet, Plate, Billet | |
Dureza Brinell | 411.0 Show Material materials with Dureza Brinell of 411.0 | Sheet, Plate, Billet | |
Dureza Rockwell C | 44.0 [-] Show Material materials with Dureza Rockwell C of 44.0 [-] | Sheet, Plate, Billet | |
Dureza Vickers | 430.0 Show Material materials with Dureza Vickers of 430.0 | Sheet, Plate, Billet | |
Elongación | 10.0 % Show Material materials with Elongación of 10.0 % | Sheet, Plate, Billet | |
Límite elástico | 965.0 MPa Show Material materials with Límite elástico of 965.0 MPa | Billet | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 |
1210.0 MPa Show Material materials with Límite elástico of 1210.0 MPa | Sheet, Plate, Billet | ||
Módulo de cizallamiento | 45.0 GPa Show Material materials with Módulo de cizallamiento of 45.0 GPa | Sheet, Plate, Billet | |
Módulo elástico | 114 GPa Show Material materials with Módulo elástico of 114 GPa | Billet | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 |
117.0 GPa Show Material materials with Módulo elástico of 117.0 GPa | Sheet, Plate, Billet | ||
Resistencia a la tracción | 1034.0 MPa Show Material materials with Resistencia a la tracción of 1034.0 MPa | Billet | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 |
1280.0 MPa Show Material materials with Resistencia a la tracción of 1280.0 MPa | Sheet, Plate, Billet | ||
Resistencia al choque, ensayo Charpy entallado | 16.0 - 19.0 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 16.0 - 19.0 kJ/m² | Billet | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 |
Aplicaciones térmicas
Property | Temperature | Value | Related Standards | Shape |
---|---|---|---|---|
Calor específico | 635 J/(kg·K) Show Material materials with Calor específico of 635 J/(kg·K) | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
Coeficiente de dilatación térmica | 20 °C | 0.000009 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000009 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
20 °C | 0.0000093 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000093 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
20 °C | 0.0000095 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000095 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
100 °C | 0.000009 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000009 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
315 °C | 0.0000093 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000093 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
538 °C | 0.0000095 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000095 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
Conductividad térmica | 5.5 W/(m·K) Show Material materials with Conductividad térmica of 5.5 W/(m·K) | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
6.6 W/(m·K) Show Material materials with Conductividad térmica of 6.6 W/(m·K) | Sheet, Plate, Billet | |||
Temperatura de fusión | 1627.0 - 1649.0 °C Show Material materials with Temperatura de fusión of 1627.0 - 1649.0 °C | Sheet, Plate, Billet | ||
1650.0 °C Show Material materials with Temperatura de fusión of 1650.0 °C | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
Eléctrico
Property | Value | Related Standards | Shape |
---|---|---|---|
Resistividad eléctrica | 1.57e-06 Ω·m Show Material materials with Resistividad eléctrica of 1.57e-06 Ω·m | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 5.0 - 6.0 % Show Material materials with Aluminio of 5.0 - 6.0 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Carbono | 0.05 Show Material materials with Carbono of 0.05 | Sheet, Plate, Billet | |
0.08 Show Material materials with Carbono of 0.08 | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
Cobre | 0.35 - 1.0 % Show Material materials with Cobre of 0.35 - 1.0 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
Estaño | 1.5 - 2.5 % Show Material materials with Estaño of 1.5 - 2.5 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Hidrógeno | 0.0125 Show Material materials with Hidrógeno of 0.0125 | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
0.015 Show Material materials with Hidrógeno of 0.015 | Sheet, Plate, Billet | ||
Hierro | 0.35 - 1.0 % Show Material materials with Hierro of 0.35 - 1.0 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Nitrógeno | 0.04 Show Material materials with Nitrógeno of 0.04 | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Oxígeno | 0.2 Show Material materials with Oxígeno of 0.2 | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Vanadio | 5.0 - 6.0 % Show Material materials with Vanadio of 5.0 - 6.0 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |