General
Property | Value | Shape |
---|---|---|
Densidad | 4.76 g/cm³ Show Material materials with Densidad of 4.76 g/cm³ | Sheet, Plate |
Medidas
Property | Value | Shape |
---|---|---|
Ancho | 400 mm Show Material materials with Ancho of 400 mm | Sheet |
600 mm Show Material materials with Ancho of 600 mm | Plate | |
1524 mm Show Material materials with Ancho of 1524 mm | Sheet | |
1600 mm Show Material materials with Ancho of 1600 mm | Plate | |
Longitud | 1500 mm Show Material materials with Longitud of 1500 mm | Sheet, Plate |
5000 mm Show Material materials with Longitud of 5000 mm | Sheet | |
6500 mm Show Material materials with Longitud of 6500 mm | Plate |
valueMetaData
Property | Value |
---|
Mecánica
Property | Value | Shape |
---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Sheet, Plate |
Dureza Rockwell B | 95.0 Show Material materials with Dureza Rockwell B of 95.0 | Sheet, Plate |
Elongación | 22.0 % Show Material materials with Elongación of 22.0 % | Sheet, Plate |
Límite elástico | 770.0 MPa Show Material materials with Límite elástico of 770.0 MPa | Sheet, Plate |
Módulo de cizallamiento | 30.8 GPa Show Material materials with Módulo de cizallamiento of 30.8 GPa | Sheet, Plate |
Módulo elástico | 82.0 GPa Show Material materials with Módulo elástico of 82.0 GPa | Sheet, Plate |
Resistencia a la tracción | 790.0 MPa Show Material materials with Resistencia a la tracción of 790.0 MPa | Sheet, Plate |
Aplicaciones térmicas
Property | Value | Shape | Comment |
---|---|---|---|
Calor específico | 490.0 - 580.0 J/(kg·K) Show Material materials with Calor específico of 490.0 - 580.0 J/(kg·K) | Typical for Titanium Beta Alloy | |
Coeficiente de dilatación térmica | 7.099999999999997e-06 - 9.699999999999999e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 7.099999999999997e-06 - 9.699999999999999e-06 1/K | Typical for Titanium Beta Alloy | |
Conductividad térmica | 8.08 W/(m·K) Show Material materials with Conductividad térmica of 8.08 W/(m·K) | Sheet, Plate | |
Temperatura de fusión | 1550.0 - 1815.0 °C Show Material materials with Temperatura de fusión of 1550.0 - 1815.0 °C | Typical for Titanium Beta Alloy |
Chemical properties