General
Property | Value | Shape |
---|---|---|
Densidad | 4.5 g/cm³ Show Material materials with Densidad of 4.5 g/cm³ | Bar |
Medidas
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | Bar | |
Diámetro | 7 mm Show Material materials with Diámetro of 7 mm | Bar | ||
115 mm Show Material materials with Diámetro of 115 mm | Bar | |||
Longitud | 6000 mm Show Material materials with Longitud of 6000 mm | Bar | max |
Mecánica
Property | Value | Shape | Comment |
---|---|---|---|
Elongación | 6.0 - 10.0 % Show Material materials with Elongación of 6.0 - 10.0 % | Bar | |
Módulo elástico | 100.0 - 120.0 GPa Show Material materials with Módulo elástico of 100.0 - 120.0 GPa | Typical for Titanium Alpha Beta Alloy | |
Resistencia a la tracción | 930.0 - 1230.0 MPa Show Material materials with Resistencia a la tracción of 930.0 - 1230.0 MPa | Bar |
Aplicaciones térmicas
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Calor específico | 200 °C | 502 J/(kg·K) Show Material materials with Calor específico of 502 J/(kg·K) | Bar | |
Coeficiente de dilatación térmica | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | ||
Conductividad térmica | 8.01 W/(m·K) Show Material materials with Conductividad térmica of 8.01 W/(m·K) | Bar | ||
Temperatura de fusión | 1500.0 - 1750.0 °C Show Material materials with Temperatura de fusión of 1500.0 - 1750.0 °C | Typical for Titanium Alpha Beta Alloy |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminio | 5.5 - 7.0 % Show Material materials with Aluminio of 5.5 - 7.0 % | Bar |
Carbono | 0.1 Show Material materials with Carbono of 0.1 | Bar |
Circonio | 0.5 Show Material materials with Circonio of 0.5 | Bar |
Cromo | 0.8 - 2.0 % Show Material materials with Cromo of 0.8 - 2.0 % | Bar |
Hidrógeno | 0.015 Show Material materials with Hidrógeno of 0.015 | Bar |
Hierro | 0.2 - 0.7 % Show Material materials with Hierro of 0.2 - 0.7 % | Bar |
Molibdeno | 2.0 - 3.0 % Show Material materials with Molibdeno of 2.0 - 3.0 % | Bar |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | Bar |
Oxígeno | 0.15 Show Material materials with Oxígeno of 0.15 | Bar |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % | Bar |