General
Property | Value | Comment |
---|---|---|
Densidad | 4.506 g/cm³ Show Material materials with Densidad of 4.506 g/cm³ | Typical for Titanium |
Medidas
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | Bar | |
Diámetro | 7 mm Show Material materials with Diámetro of 7 mm | Bar | ||
115 mm Show Material materials with Diámetro of 115 mm | Bar | |||
Longitud | 6000 mm Show Material materials with Longitud of 6000 mm | Bar | max |
Mecánica
Property | Value | Shape | Comment |
---|---|---|---|
Elongación | 10.0 % Show Material materials with Elongación of 10.0 % | Bar | |
Módulo elástico | 100.0 - 120.0 GPa Show Material materials with Módulo elástico of 100.0 - 120.0 GPa | Typical for Titanium Alpha Alloy | |
Resistencia a la tracción | 880.0 - 1080.0 MPa Show Material materials with Resistencia a la tracción of 880.0 - 1080.0 MPa | Bar |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 460.0 - 527.0 J/(kg·K) Show Material materials with Calor específico of 460.0 - 527.0 J/(kg·K) | Typical for Titanium Alpha Alloy |
Coeficiente de dilatación térmica | 7.599999999999997e-06 - 1.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 7.599999999999997e-06 - 1.1e-05 1/K | Typical for Titanium Alpha Alloy |
Conductividad térmica | 4.0 - 17.0 W/(m·K) Show Material materials with Conductividad térmica of 4.0 - 17.0 W/(m·K) | Typical for Titanium Alpha Alloy |
Temperatura de fusión | 1540.0 - 1715.0 °C Show Material materials with Temperatura de fusión of 1540.0 - 1715.0 °C | Typical for Titanium Alpha Alloy |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminio | 6.2 - 7.3 % Show Material materials with Aluminio of 6.2 - 7.3 % | Bar |
Carbono | 0.1 Show Material materials with Carbono of 0.1 | Bar |
Circonio | 3.5 - 4.5 % Show Material materials with Circonio of 3.5 - 4.5 % | Bar |
Estaño | 2.0 - 3.0 % Show Material materials with Estaño of 2.0 - 3.0 % | Bar |
Hidrógeno | 0.015 Show Material materials with Hidrógeno of 0.015 | Bar |
Hierro | 0.2 Show Material materials with Hierro of 0.2 | Bar |
Molibdeno | 0.4 - 1.0 % Show Material materials with Molibdeno of 0.4 - 1.0 % | Bar |
Niobio | 0.5 - 1.5 % Show Material materials with Niobio of 0.5 - 1.5 % | Bar |
Nitrógeno | 0.04 Show Material materials with Nitrógeno of 0.04 | Bar |
Oxígeno | 0.14 Show Material materials with Oxígeno of 0.14 | Bar |
Silicona | 0.1 - 0.25 % Show Material materials with Silicona of 0.1 - 0.25 % | Bar |