General
Property | Value | Shape |
---|---|---|
Densidad | 4.55 g/cm³ Show Material materials with Densidad of 4.55 g/cm³ | Bar |
Medidas
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | Bar | |
Diámetro | 7 mm Show Material materials with Diámetro of 7 mm | Bar | ||
115 mm Show Material materials with Diámetro of 115 mm | Bar | |||
Longitud | 6000 mm Show Material materials with Longitud of 6000 mm | Bar | max |
Mecánica
Property | Value | Shape | Comment |
---|---|---|---|
Elongación | 8.0 - 11.0 % Show Material materials with Elongación of 8.0 - 11.0 % | Bar | |
Módulo elástico | 100.0 - 120.0 GPa Show Material materials with Módulo elástico of 100.0 - 120.0 GPa | Typical for Titanium Alpha Alloy | |
Resistencia a la tracción | 635.0 - 885.0 MPa Show Material materials with Resistencia a la tracción of 635.0 - 885.0 MPa | Bar |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 460.0 - 527.0 J/(kg·K) Show Material materials with Calor específico of 460.0 - 527.0 J/(kg·K) | Typical for Titanium Alpha Alloy |
Coeficiente de dilatación térmica | 7.599999999999997e-06 - 1.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 7.599999999999997e-06 - 1.1e-05 1/K | Typical for Titanium Alpha Alloy |
Conductividad térmica | 4.0 - 17.0 W/(m·K) Show Material materials with Conductividad térmica of 4.0 - 17.0 W/(m·K) | Typical for Titanium Alpha Alloy |
Temperatura de fusión | 1540.0 - 1715.0 °C Show Material materials with Temperatura de fusión of 1540.0 - 1715.0 °C | Typical for Titanium Alpha Alloy |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminio | 3.5 - 5.0 % Show Material materials with Aluminio of 3.5 - 5.0 % | Bar |
Carbono | 0.1 Show Material materials with Carbono of 0.1 | Bar |
Circonio | 0.3 Show Material materials with Circonio of 0.3 | Bar |
Hidrógeno | 0.012 Show Material materials with Hidrógeno of 0.012 | Bar |
Hierro | 0.3 Show Material materials with Hierro of 0.3 | Bar |
Manganeso | 0.8 - 2.0 % Show Material materials with Manganeso of 0.8 - 2.0 % | Bar |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | Bar |
Oxígeno | 0.15 Show Material materials with Oxígeno of 0.15 | Bar |
Silicona | 0.12 Show Material materials with Silicona of 0.12 | Bar |