General
Property | Value | Shape |
---|---|---|
Densidad | 4.48 g/cm³ Show Material materials with Densidad of 4.48 g/cm³ | Sheet, Billet, Tube |
Medidas
Property | Value | Shape |
---|---|---|
Ancho | 400 mm Show Material materials with Ancho of 400 mm | Sheet |
600 mm Show Material materials with Ancho of 600 mm | Sheet | |
1524 mm Show Material materials with Ancho of 1524 mm | Sheet | |
1600 mm Show Material materials with Ancho of 1600 mm | Sheet | |
Diámetro | 5 mm Show Material materials with Diámetro of 5 mm | Tube |
25.4 mm Show Material materials with Diámetro of 25.4 mm | Billet | |
125 mm Show Material materials with Diámetro of 125 mm | Billet | |
130 mm Show Material materials with Diámetro of 130 mm | Tube | |
Longitud | 1000 mm Show Material materials with Longitud of 1000 mm | Tube |
1500 mm Show Material materials with Longitud of 1500 mm | Sheet | |
5000 mm Show Material materials with Longitud of 5000 mm | Sheet, Tube | |
6500 mm Show Material materials with Longitud of 6500 mm | Sheet | |
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | Tube |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | Billet |
valueMetaData
Property | Value |
---|
Mecánica
Property | Value | Shape |
---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Billet, Tube |
Dureza Brinell | 256.0 Show Material materials with Dureza Brinell of 256.0 | Billet, Tube |
Dureza Rockwell C | 24.0 [-] Show Material materials with Dureza Rockwell C of 24.0 [-] | Billet, Tube |
Dureza Vickers | 280.0 Show Material materials with Dureza Vickers of 280.0 | Billet, Tube |
Elongación | 15.0 % Show Material materials with Elongación of 15.0 % | Billet |
Límite elástico | 520.0 MPa Show Material materials with Límite elástico of 520.0 MPa | Sheet, Billet, Tube |
Módulo de cizallamiento | 44.0 GPa Show Material materials with Módulo de cizallamiento of 44.0 GPa | Billet, Tube |
Módulo elástico | 103.0 GPa Show Material materials with Módulo elástico of 103.0 GPa | Sheet, Billet, Tube |
Resistencia a la tracción | 620.0 MPa Show Material materials with Resistencia a la tracción of 620.0 MPa | Sheet, Billet, Tube |
Aplicaciones térmicas
Property | Value | Shape | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Titanium | |
Conductividad térmica | 8.3 W/(m·K) Show Material materials with Conductividad térmica of 8.3 W/(m·K) | Sheet, Billet, Tube | |
Temperatura de fusión | 1700.0 °C Show Material materials with Temperatura de fusión of 1700.0 °C | Billet, Tube |