General
Property | Value | Shape |
---|---|---|
Densidad | 4.49 g/cm³ Show Material materials with Densidad of 4.49 g/cm³ | Tube |
Medidas
Property | Value | Shape |
---|---|---|
Diámetro | 5 mm Show Material materials with Diámetro of 5 mm | Tube |
25.4 mm Show Material materials with Diámetro of 25.4 mm | Billet | |
125 mm Show Material materials with Diámetro of 125 mm | Billet | |
130 mm Show Material materials with Diámetro of 130 mm | Tube | |
Longitud | 1000 mm Show Material materials with Longitud of 1000 mm | Tube |
5000 mm Show Material materials with Longitud of 5000 mm | Tube | |
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | Tube |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | Billet |
Mecánica
Property | Value | Shape | Comment |
---|---|---|---|
Elongación | 15.0 - 25.0 % Show Material materials with Elongación of 15.0 - 25.0 % | Tube | |
Módulo elástico | 100.0 - 120.0 GPa Show Material materials with Módulo elástico of 100.0 - 120.0 GPa | Typical for Low Alloy Titanium | |
Resistencia a la tracción | 480.0 - 680.0 MPa Show Material materials with Resistencia a la tracción of 480.0 - 680.0 MPa | Tube |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 515.0 - 597.0 J/(kg·K) Show Material materials with Calor específico of 515.0 - 597.0 J/(kg·K) | Typical for Low Alloy Titanium |
Coeficiente de dilatación térmica | 7.599999999999997e-06 - 9.9e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 7.599999999999997e-06 - 9.9e-06 1/K | Typical for Low Alloy Titanium |
Conductividad térmica | 15.0 - 22.0 W/(m·K) Show Material materials with Conductividad térmica of 15.0 - 22.0 W/(m·K) | Typical for Low Alloy Titanium |
Temperatura de fusión | 1650.0 - 1705.0 °C Show Material materials with Temperatura de fusión of 1650.0 - 1705.0 °C | Typical for Low Alloy Titanium |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminio | 0.2 - 0.7 % Show Material materials with Aluminio of 0.2 - 0.7 % | Billet, Tube |
Carbono | 0.07 Show Material materials with Carbono of 0.07 | Billet, Tube |
Circonio | 0.3 Show Material materials with Circonio of 0.3 | Billet, Tube |
Nitrógeno | 0.04 Show Material materials with Nitrógeno of 0.04 | Billet, Tube |
Oxígeno | 0.12 Show Material materials with Oxígeno of 0.12 | Billet, Tube |
Silicona | 0.1 Show Material materials with Silicona of 0.1 | Billet, Tube |