General
Property | Value | Related Standards | Shape |
---|---|---|---|
Densidad | 4.51 g/cm³ Show Material materials with Densidad of 4.51 g/cm³ | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Medidas
Property | Value | Related Standards | Shape |
---|---|---|---|
Diámetro | 25.4 mm Show Material materials with Diámetro of 25.4 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
125 mm Show Material materials with Diámetro of 125 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
Wall thickness | 2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elongación | 10.0 - 30.0 % Show Material materials with Elongación of 10.0 - 30.0 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
Módulo elástico | 100.0 - 120.0 GPa Show Material materials with Módulo elástico of 100.0 - 120.0 GPa | Typical for Titanium Alpha Alloy | ||
Resistencia a la tracción | 440.0 - 637.0 MPa Show Material materials with Resistencia a la tracción of 440.0 - 637.0 MPa | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 460.0 - 527.0 J/(kg·K) Show Material materials with Calor específico of 460.0 - 527.0 J/(kg·K) | Typical for Titanium Alpha Alloy |
Coeficiente de dilatación térmica | 7.599999999999997e-06 - 1.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 7.599999999999997e-06 - 1.1e-05 1/K | Typical for Titanium Alpha Alloy |
Conductividad térmica | 4.0 - 17.0 W/(m·K) Show Material materials with Conductividad térmica of 4.0 - 17.0 W/(m·K) | Typical for Titanium Alpha Alloy |
Temperatura de fusión | 1540.0 - 1715.0 °C Show Material materials with Temperatura de fusión of 1540.0 - 1715.0 °C | Typical for Titanium Alpha Alloy |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 0.4 - 1.4 % Show Material materials with Aluminio of 0.4 - 1.4 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Carbono | 0.1 Show Material materials with Carbono of 0.1 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Circonio | 0.3 Show Material materials with Circonio of 0.3 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Hidrógeno | 0.012 Show Material materials with Hidrógeno of 0.012 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Hierro | 0.3 Show Material materials with Hierro of 0.3 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Manganeso | 0.5 - 1.3 % Show Material materials with Manganeso of 0.5 - 1.3 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Oxígeno | 0.15 Show Material materials with Oxígeno of 0.15 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Silicona | 0.12 Show Material materials with Silicona of 0.12 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |