General
Property | Value | Related Standards | Shape |
---|---|---|---|
Densidad | 4.505 g/cm³ Show Material materials with Densidad of 4.505 g/cm³ | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
4.55 g/cm³ Show Material materials with Densidad of 4.55 g/cm³ | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
Medidas
Property | Value | Related Standards | Shape |
---|---|---|---|
Diámetro | 5 mm Show Material materials with Diámetro of 5 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
25.4 mm Show Material materials with Diámetro of 25.4 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
125 mm Show Material materials with Diámetro of 125 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
130 mm Show Material materials with Diámetro of 130 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube | |
Longitud | 1000 mm Show Material materials with Longitud of 1000 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
5000 mm Show Material materials with Longitud of 5000 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube | |
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.361 [-] Show Material materials with Coeficiente de Poisson of 0.361 [-] | Typical for Pure Titanium | ||
Elongación | 6.0 - 20.0 % Show Material materials with Elongación of 6.0 - 20.0 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube | |
10.0 - 30.0 % Show Material materials with Elongación of 10.0 - 30.0 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | ||
Módulo de cizallamiento | 46.0 GPa Show Material materials with Módulo de cizallamiento of 46.0 GPa | Typical for Pure Titanium | ||
Módulo elástico | 120.0 GPa Show Material materials with Módulo elástico of 120.0 GPa | Typical for Pure Titanium | ||
Resistencia a la tracción | 295.0 - 590.0 MPa Show Material materials with Resistencia a la tracción of 295.0 - 590.0 MPa | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
635.0 - 885.0 MPa Show Material materials with Resistencia a la tracción of 635.0 - 885.0 MPa | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
Aplicaciones térmicas
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Calor específico | 540 J/(kg·K) Show Material materials with Calor específico of 540 J/(kg·K) | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube | |
Coeficiente de dilatación térmica | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | ||
Conductividad térmica | 18.85 W/(m·K) Show Material materials with Conductividad térmica of 18.85 W/(m·K) | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube | |
Temperatura de fusión | 1668.0 °C Show Material materials with Temperatura de fusión of 1668.0 °C | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Carbono | 0.07 Show Material materials with Carbono of 0.07 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Hidrógeno | 0.01 Show Material materials with Hidrógeno of 0.01 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Hierro | 0.25 Show Material materials with Hierro of 0.25 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Nitrógeno | 0.04 Show Material materials with Nitrógeno of 0.04 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Oxígeno | 0.2 Show Material materials with Oxígeno of 0.2 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Silicona | 0.1 Show Material materials with Silicona of 0.1 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |