General
Property | Value | Related Standards | Shape |
---|---|---|---|
Densidad | 4.51 g/cm³ Show Material materials with Densidad of 4.51 g/cm³ | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
4.55 g/cm³ Show Material materials with Densidad of 4.55 g/cm³ | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Medidas
Property | Value | Related Standards | Shape |
---|---|---|---|
Diámetro | 5 mm Show Material materials with Diámetro of 5 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
25.4 mm Show Material materials with Diámetro of 25.4 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
125 mm Show Material materials with Diámetro of 125 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
130 mm Show Material materials with Diámetro of 130 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube | |
Longitud | 1000 mm Show Material materials with Longitud of 1000 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
5000 mm Show Material materials with Longitud of 5000 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube | |
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elongación | 8.0 - 25.0 % Show Material materials with Elongación of 8.0 - 25.0 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
10.0 - 30.0 % Show Material materials with Elongación of 10.0 - 30.0 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube | ||
Módulo elástico | 100.0 - 120.0 GPa Show Material materials with Módulo elástico of 100.0 - 120.0 GPa | Typical for Titanium Alpha Alloy | ||
Resistencia a la tracción | 440.0 - 637.0 MPa Show Material materials with Resistencia a la tracción of 440.0 - 637.0 MPa | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube | |
540.0 - 735.0 MPa Show Material materials with Resistencia a la tracción of 540.0 - 735.0 MPa | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Aplicaciones térmicas
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Calor específico | 200 °C | 565 J/(kg·K) Show Material materials with Calor específico of 565 J/(kg·K) | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube | |
Coeficiente de dilatación térmica | 7.599999999999997e-06 - 1.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 7.599999999999997e-06 - 1.1e-05 1/K | Typical for Titanium Alpha Alloy | |||
Conductividad térmica | 9.63 W/(m·K) Show Material materials with Conductividad térmica of 9.63 W/(m·K) | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube | ||
Temperatura de fusión | 1540.0 - 1715.0 °C Show Material materials with Temperatura de fusión of 1540.0 - 1715.0 °C | Typical for Titanium Alpha Alloy |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 1.5 - 2.5 % Show Material materials with Aluminio of 1.5 - 2.5 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Carbono | 0.1 Show Material materials with Carbono of 0.1 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Circonio | 0.3 Show Material materials with Circonio of 0.3 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Hidrógeno | 0.012 Show Material materials with Hidrógeno of 0.012 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Hierro | 0.3 Show Material materials with Hierro of 0.3 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Manganeso | 0.7 - 2.0 % Show Material materials with Manganeso of 0.7 - 2.0 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Oxígeno | 0.15 Show Material materials with Oxígeno of 0.15 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Silicona | 0.12 Show Material materials with Silicona of 0.12 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |