General
Property | Value |
---|---|
Densidad | 0.95 - 1.33 g/cm³ Show Material materials with Densidad of 0.95 - 1.33 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 100.0 - 700.0 % Show Material materials with Elongación of 100.0 - 700.0 % | |
Resistencia a la tracción | 7.0 - 38.0 MPa Show Material materials with Resistencia a la tracción of 7.0 - 38.0 MPa | at 100-700% strain |
Aplicaciones térmicas
Property | Value |
---|---|
Coeficiente de dilatación térmica | 0.000195 - 0.00026 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000195 - 0.00026 1/K |
Óptico
Property | Value |
---|---|
Transparencia | no |
Technological properties
Property | ||
---|---|---|
Application areas | Oil production equipment, fuel hoses, in-tank insulators, refrigerant hoses, O-rings | |
Processing methods | Compression molding, extrusion, vulcanization |