General
Property | Value |
---|---|
Densidad | 0.03 - 0.09 g/cm³ Show Material materials with Densidad of 0.03 - 0.09 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 4.0 - 5.0 % Show Material materials with Elongación of 4.0 - 5.0 % | |
Resistencia a la tracción | 0.2 - 0.9 MPa Show Material materials with Resistencia a la tracción of 0.2 - 0.9 MPa | at 4-5% strain |
Aplicaciones térmicas
Property | Value |
---|---|
Conductividad térmica | 0.02 - 0.03 W/(m·K) Show Material materials with Conductividad térmica of 0.02 - 0.03 W/(m·K) |
Óptico
Property | Value |
---|---|
Transparencia | no |
Technological properties
Property | ||
---|---|---|
Application areas | Insulation applications, automotive interiors | |
Processing methods | Foaming |