General
Property | Value |
---|---|
Densidad | 1.11 - 1.15 g/cm³ Show Material materials with Densidad of 1.11 - 1.15 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 2.0 - 7.0 % Show Material materials with Elongación of 2.0 - 7.0 % | |
Módulo elástico | 3.0 - 4.0 GPa Show Material materials with Módulo elástico of 3.0 - 4.0 GPa | |
Resistencia a la tracción | 60.0 - 95.0 MPa Show Material materials with Resistencia a la tracción of 60.0 - 95.0 MPa | at 2-7% strain |
Resistencia al choque, ensayo Charpy no entallado | 15 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 15 kJ/m² | |
30 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 30 kJ/m² |
Aplicaciones térmicas
Property | Value |
---|
Óptico
Property | Value |
---|---|
Transparencia | no |
Technological properties
Property | ||
---|---|---|
Application areas | Corrosion resistance parts, tanks relining, marine and swimming pool applications | |
Processing methods | Compression molding |