General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.75 - 1.5 % Show Material materials with Aluminio of 0.75 - 1.5 % | |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | |
Carbono | 0.09 % Show Material materials with Carbono of 0.09 % | |
Cromo | 16 - 18 % Show Material materials with Cromo of 16 - 18 % | |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % | |
Hierro | 70.58 - 76.75 % Show Material materials with Hierro of 70.58 - 76.75 % | balance |
Manganeso | 1 % Show Material materials with Manganeso of 1 % | |
Níquel | 6.5 - 7.75 % Show Material materials with Níquel of 6.5 - 7.75 % | |
Silicona | 1 % Show Material materials with Silicona of 1 % |