General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Módulo elástico | 190.0 - 210.0 GPa Show Material materials with Módulo elástico of 190.0 - 210.0 GPa | Typical for Steel |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Azufre | 0.035 - 0.05 % Show Material materials with Azufre of 0.035 - 0.05 % | SAE J407 |
Boro | 0.0005 % Show Material materials with Boro of 0.0005 % | SAE J407 |
Carbono | 0.12 - 0.18 % Show Material materials with Carbono of 0.12 - 0.18 % | SAE J407 |
Cobre | 0.35 Show Material materials with Cobre of 0.35 | SAE J407 |
Cromo | 0.25 - 0.55 % Show Material materials with Cromo of 0.25 - 0.55 % | SAE J407 |
Fósforo | 0.035 Show Material materials with Fósforo of 0.035 | SAE J407 |
Hierro | 99.9949 - 99.9989 % Show Material materials with Hierro of 99.9949 - 99.9989 % | SAE J407 |
Manganeso | 0.7 - 1.05 % Show Material materials with Manganeso of 0.7 - 1.05 % | SAE J407 |
Molibdeno | 0.08 - 0.15 % Show Material materials with Molibdeno of 0.08 - 0.15 % | SAE J407 |
Níquel | 0.25 - 0.65 % Show Material materials with Níquel of 0.25 - 0.65 % | SAE J407 |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % | SAE J407 |