Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Molybdenum Steel |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Molybdenum Steel |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 456 J/(kg·K) Show Material materials with Calor específico of 456 J/(kg·K) | Typical for Molybdenum Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.29E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.29E-5 1/K | Typical for Molybdenum Steel |
Conductividad térmica | 23.0 °C | 37 - 48 W/(m·K) Show Material materials with Conductividad térmica of 37 - 48 W/(m·K) | Typical for Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.4 - 0.45 % Show Material materials with Carbono of 0.4 - 0.45 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | 97.97 - 98.55 % Show Material materials with Hierro of 97.97 - 98.55 % |
Manganeso | 0.7 - 0.9 % Show Material materials with Manganeso of 0.7 - 0.9 % |
Molibdeno | 0.2 - 0.3 % Show Material materials with Molibdeno of 0.2 - 0.3 % |
Silicona | 0.15 - 0.3 % Show Material materials with Silicona of 0.15 - 0.3 % |