General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Carbono | 0.04 % Show Material materials with Carbono of 0.04 % |
Cobre | 3.3 % Show Material materials with Cobre of 3.3 % |
Cromo | 16 % Show Material materials with Cromo of 16 % |
Hierro | 69.91 - 78.35 % Show Material materials with Hierro of 69.91 - 78.35 % |
Manganeso | 0.28 % Show Material materials with Manganeso of 0.28 % |
Niobio | 0.27 % Show Material materials with Niobio of 0.27 % |
Níquel | 4.25 % Show Material materials with Níquel of 4.25 % |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % |