General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 5 % Show Material materials with Aluminio of 5 % |
Boro | 0.015 % Show Material materials with Boro of 0.015 % |
Carbono | 0.15 % Show Material materials with Carbono of 0.15 % |
Circonio | 0.05 % Show Material materials with Circonio of 0.05 % |
Cobalto | 10 % Show Material materials with Cobalto of 10 % |
Cromo | 9 % Show Material materials with Cromo of 9 % |
Hierro | 60.28 - 100 % Show Material materials with Hierro of 60.28 - 100 % |
Niobio | 1 % Show Material materials with Niobio of 1 % |
Titanio | 2 % Show Material materials with Titanio of 2 % |
Wolframio | 12.5 % Show Material materials with Wolframio of 12.5 % |