General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 1.17 % Show Material materials with Aluminio of 1.17 % |
Carbono | 0.07 % Show Material materials with Carbono of 0.07 % |
Cromo | 15 % Show Material materials with Cromo of 15 % |
Hierro | 69.59 - 76.75 % Show Material materials with Hierro of 69.59 - 76.75 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 2.2 % Show Material materials with Molibdeno of 2.2 % |
Níquel | 7 % Show Material materials with Níquel of 7 % |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |