General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.95 - 1.3 % Show Material materials with Aluminio of 0.95 - 1.3 % |
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.38 - 0.43 % Show Material materials with Carbono of 0.38 - 0.43 % |
Cromo | 1.4 - 1.8 % Show Material materials with Cromo of 1.4 - 1.8 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 95.02 - 96.32 % Show Material materials with Hierro of 95.02 - 96.32 % |
Manganeso | 0.5 - 0.7 % Show Material materials with Manganeso of 0.5 - 0.7 % |
Silicona | 0.15 - 0.3 % Show Material materials with Silicona of 0.15 - 0.3 % |
Vanadio | 0.3 - 0.4 % Show Material materials with Vanadio of 0.3 - 0.4 % |