General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.6 - 7.8 g/cm³ Show Material materials with Densidad of 7.6 - 7.8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Límite elástico | 23.0 °C | 553 - 700 MPa Show Material materials with Límite elástico of 553 - 700 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 23.0 °C | 195 GPa Show Material materials with Módulo elástico of 195 GPa | Typical for Austenitic Stainless Steel |
Resistencia a la tracción | 23.0 °C | 862 - 1155 MPa Show Material materials with Resistencia a la tracción of 862 - 1155 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Coeficiente de dilatación térmica | 200.0 °C | 1.44E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.44E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
700.0 °C | 1.75E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.85E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.85E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Conductividad térmica | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Conductividad térmica of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | |
Carbono | 0.5 - 0.6 % Show Material materials with Carbono of 0.5 - 0.6 % | |
Cromo | 19.5 - 21.5 % Show Material materials with Cromo of 19.5 - 21.5 % | |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % | |
Hierro | 65 - 71.55 % Show Material materials with Hierro of 65 - 71.55 % | Balance |
Manganeso | 7 - 10 % Show Material materials with Manganeso of 7 - 10 % | |
Nitrógeno | 0.2 - 0.4 % Show Material materials with Nitrógeno of 0.2 - 0.4 % | |
Níquel | 1.5 - 2.75 % Show Material materials with Níquel of 1.5 - 2.75 % | |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % |