Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.9 - 8.2 g/cm³ Show Material materials with Densidad of 7.9 - 8.2 g/cm³ | Typical for Austenitic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Dureza Rockwell C | 23.0 °C | 35 [-] Show Material materials with Dureza Rockwell C of 35 [-] | |
Elongación A5 | 23.0 °C | 57 % Show Material materials with Elongación A5 of 57 % | |
Estricción | 23.0 °C | 5 % Show Material materials with Estricción of 5 % | |
Límite elástico | 23.0 °C | 520 MPa Show Material materials with Límite elástico of 520 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 23.0 °C | 195 GPa Show Material materials with Módulo elástico of 195 GPa | Typical for Austenitic Stainless Steel |
Resistencia a la tracción | 23.0 °C | 1080 MPa Show Material materials with Resistencia a la tracción of 1080 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 1.9E-5 1/K | Typical for Austenitic Stainless Steel |
Conductividad térmica | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Conductividad térmica of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % | |
Carbono | 0.47 - 0.57 % Show Material materials with Carbono of 0.47 - 0.57 % | |
Cromo | 20 - 22 % Show Material materials with Cromo of 20 - 22 % | |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % | |
Hierro | 60.43 - 65.83 % Show Material materials with Hierro of 60.43 - 65.83 % | Balance |
Manganeso | 11 - 13 % Show Material materials with Manganeso of 11 - 13 % | |
Nitrógeno | 0.4 - 0.5 % Show Material materials with Nitrógeno of 0.4 - 0.5 % | |
Silicona | 2 - 3 % Show Material materials with Silicona of 2 - 3 % |