General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Estricción | 20.0 °C | 61 % Show Material materials with Estricción of 61 % | |
650.0 °C | 60 % Show Material materials with Estricción of 60 % | ||
760.0 °C | 60 % Show Material materials with Estricción of 60 % | ||
Límite elástico | 20.0 °C | 480 MPa Show Material materials with Límite elástico of 480 MPa | |
650.0 °C | 220 MPa Show Material materials with Límite elástico of 220 MPa | ||
760.0 °C | 190 MPa Show Material materials with Límite elástico of 190 MPa | ||
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 880 MPa Show Material materials with Resistencia a la tracción of 880 MPa | |
650.0 °C | 490 MPa Show Material materials with Resistencia a la tracción of 490 MPa | ||
760.0 °C | 320 MPa Show Material materials with Resistencia a la tracción of 320 MPa | ||
Chemical properties
Property | Value |
---|---|
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % |
Cromo | 21 % Show Material materials with Cromo of 21 % |
Hierro | 66.2 - 100 % Show Material materials with Hierro of 66.2 - 100 % |
Manganeso | 6.5 % Show Material materials with Manganeso of 6.5 % |
Nitrógeno | 0.2 % Show Material materials with Nitrógeno of 0.2 % |
Níquel | 5.5 % Show Material materials with Níquel of 5.5 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |