General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.69 g/cm³ Show Material materials with Densidad of 7.69 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Dureza Brinell | 760.0 °C | 120 [-] Show Material materials with Dureza Brinell of 120 [-] | |
Elongación | 23.0 °C | 34.2 % Show Material materials with Elongación of 34.2 % | |
Estricción | 20.0 °C | 26 % Show Material materials with Estricción of 26 % | |
650.0 °C | 30 % Show Material materials with Estricción of 30 % | ||
760.0 °C | 30 % Show Material materials with Estricción of 30 % | ||
Límite elástico | 20.0 °C | 520 MPa Show Material materials with Límite elástico of 520 MPa | |
650.0 °C | 310 MPa Show Material materials with Límite elástico of 310 MPa | ||
760.0 °C | 240 MPa Show Material materials with Límite elástico of 240 MPa | ||
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 23.0 °C | 195 GPa Show Material materials with Módulo elástico of 195 GPa | Typical for Austenitic Stainless Steel |
Resistencia a la tracción | 20.0 °C | 1080 MPa Show Material materials with Resistencia a la tracción of 1080 MPa | |
650.0 °C | 460 MPa Show Material materials with Resistencia a la tracción of 460 MPa | ||
760.0 °C | 28 MPa Show Material materials with Resistencia a la tracción of 28 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Coeficiente de dilatación térmica | 760.0 °C | 1.78E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.78E-5 1/K | The mentioned value is between 20°C and the mentioned temperature |
Conductividad térmica | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Conductividad térmica of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | |
Carbono | 0.3 - 0.45 % Show Material materials with Carbono of 0.3 - 0.45 % | |
Cromo | 18 - 20 % Show Material materials with Cromo of 18 - 20 % | |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % | |
Hierro | 66.5 - 70.65 % Show Material materials with Hierro of 66.5 - 70.65 % | Balance |
Manganeso | 0.8 - 1.3 % Show Material materials with Manganeso of 0.8 - 1.3 % | |
Níquel | 7.5 - 8.5 % Show Material materials with Níquel of 7.5 - 8.5 % | |
Silicona | 2.75 - 3.25 % Show Material materials with Silicona of 2.75 - 3.25 % |