General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.6 - 7.8 g/cm³ Show Material materials with Densidad of 7.6 - 7.8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Dureza Rockwell C | 23.0 °C | 30 [-] Show Material materials with Dureza Rockwell C of 30 [-] | |
Elongación A5 | 23.0 °C | 8 - 25 % Show Material materials with Elongación A5 of 8 - 25 % | |
Estricción | 23.0 °C | 9 - 10 % Show Material materials with Estricción of 9 - 10 % | |
Límite elástico | 23.0 °C | 580 - 895 MPa Show Material materials with Límite elástico of 580 - 895 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 23.0 °C | 205 GPa Show Material materials with Módulo elástico of 205 GPa | |
Resistencia a la tracción | 23.0 °C | 880 - 1200 MPa Show Material materials with Resistencia a la tracción of 880 - 1200 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.55E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.55E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
300.0 °C | 1.75E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.85E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.85E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
700.0 °C | 1.88E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.88E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Conductividad térmica | 23.0 °C | 14.5 W/(m·K) Show Material materials with Conductividad térmica of 14.5 W/(m·K) | |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | |
Carbono | 0.48 - 0.58 % Show Material materials with Carbono of 0.48 - 0.58 % | |
Cromo | 20 - 22 % Show Material materials with Cromo of 20 - 22 % | |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % | |
Hierro | 61.12 - 67.89 % Show Material materials with Hierro of 61.12 - 67.89 % | Balance |
Manganeso | 8 - 10 % Show Material materials with Manganeso of 8 - 10 % | |
Nitrógeno | 0.38 - 0.55 % Show Material materials with Nitrógeno of 0.38 - 0.55 % | |
Níquel | 3.25 - 4.5 % Show Material materials with Níquel of 3.25 - 4.5 % | |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % |