General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8 - 8.3 g/cm³ Show Material materials with Densidad of 8 - 8.3 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell C | 20.0 °C | 32 - 40 [-] Show Material materials with Dureza Rockwell C of 32 - 40 [-] |
Elongación A5 | 20.0 °C | 12 - 33 % Show Material materials with Elongación A5 of 12 - 33 % |
Estricción | 20.0 °C | 20 - 32 % Show Material materials with Estricción of 20 - 32 % |
Límite elástico | 20.0 °C | 630 - 850 MPa Show Material materials with Límite elástico of 630 - 850 MPa |
Módulo elástico | 20.0 °C | 215 GPa Show Material materials with Módulo elástico of 215 GPa |
Resistencia a la tracción | 20.0 °C | 1100 - 1300 MPa Show Material materials with Resistencia a la tracción of 1100 - 1300 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
200.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
300.0 °C | 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.45E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.45E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
600.0 °C | 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
700.0 °C | 1.55E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.55E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.49E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.49E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Conductividad térmica | 20.0 °C | 13 W/(m·K) Show Material materials with Conductividad térmica of 13 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminio | 1.1 - 1.35 % Show Material materials with Aluminio of 1.1 - 1.35 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Boro | 1.5E-3 - 9E-3 % Show Material materials with Boro of 1.5E-3 - 9E-3 % |
Carbono | 0.03 - 0.1 % Show Material materials with Carbono of 0.03 - 0.1 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cromo | 14 - 17 % Show Material materials with Cromo of 14 - 17 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 5 - 9 % Show Material materials with Hierro of 5 - 9 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 2 - 2.6 % Show Material materials with Titanio of 2 - 2.6 % |