General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8 - 8.3 g/cm³ Show Material materials with Densidad of 8 - 8.3 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell C | 20.0 °C | 32 - 38 [-] Show Material materials with Dureza Rockwell C of 32 - 38 [-] |
Elongación A5 | 20.0 °C | 15 - 40 % Show Material materials with Elongación A5 of 15 - 40 % |
Estricción | 20.0 °C | 20 - 38 % Show Material materials with Estricción of 20 - 38 % |
Límite elástico | 20.0 °C | 620 - 969 MPa Show Material materials with Límite elástico of 620 - 969 MPa |
Módulo elástico | 20.0 °C | 208 - 215 GPa Show Material materials with Módulo elástico of 208 - 215 GPa |
Resistencia a la tracción | 20.0 °C | 1050 - 1400 MPa Show Material materials with Resistencia a la tracción of 1050 - 1400 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.19E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.19E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
200.0 °C | 1.26E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.26E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
300.0 °C | 1.31E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.31E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.37E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.37E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
600.0 °C | 1.33E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.33E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
700.0 °C | 1.45E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.45E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.39E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.39E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Conductividad térmica | 20.0 °C | 13 W/(m·K) Show Material materials with Conductividad térmica of 13 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminio | 1 - 1.8 % Show Material materials with Aluminio of 1 - 1.8 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Boro | 8E-3 % Show Material materials with Boro of 8E-3 % |
Carbono | 0.04 - 0.1 % Show Material materials with Carbono of 0.04 - 0.1 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Cromo | 18 - 21 % Show Material materials with Cromo of 18 - 21 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 3 % Show Material materials with Hierro of 3 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 1.8 - 2.7 % Show Material materials with Titanio of 1.8 - 2.7 % |