General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.9 - 8 g/cm³ Show Material materials with Densidad of 7.9 - 8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell C | 20.0 °C | 32 - 37 [-] Show Material materials with Dureza Rockwell C of 32 - 37 [-] |
Elongación A5 | 20.0 °C | 25 - 35 % Show Material materials with Elongación A5 of 25 - 35 % |
Estricción | 20.0 °C | 5 - 45 % Show Material materials with Estricción of 5 - 45 % |
Límite elástico | 20.0 °C | 692 - 830 MPa Show Material materials with Límite elástico of 692 - 830 MPa |
Módulo elástico | 20.0 °C | 208 GPa Show Material materials with Módulo elástico of 208 GPa |
Resistencia a la tracción | 20.0 °C | 1103 - 1300 MPa Show Material materials with Resistencia a la tracción of 1103 - 1300 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.41E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.41E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
600.0 °C | 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.48E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.48E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1300.0 °C | 1.53E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.53E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Conductividad térmica | 20.0 °C | 13 W/(m·K) Show Material materials with Conductividad térmica of 13 W/(m·K) |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 1.1 % Show Material materials with Aluminio of 1.1 % | |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % | |
Boro | 3E-3 - 7E-3 % Show Material materials with Boro of 3E-3 - 7E-3 % | |
Carbono | 0.03 - 0.06 % Show Material materials with Carbono of 0.03 - 0.06 % | |
Cobalto | 1 % Show Material materials with Cobalto of 1 % | |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % | |
Cromo | 22.3 - 22.9 % Show Material materials with Cromo of 22.3 - 22.9 % | |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % | |
Hierro | 70.4 - 100 % Show Material materials with Hierro of 70.4 - 100 % | Balance |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % | |
Molibdeno | 1.7 - 2.3 % Show Material materials with Molibdeno of 1.7 - 2.3 % | |
Niobio | 0.75 - 0.95 % Show Material materials with Niobio of 0.75 - 0.95 % | |
Níquel | 55 - 58 % Show Material materials with Níquel of 55 - 58 % | |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % | |
Titanio | 2.1 - 2.4 % Show Material materials with Titanio of 2.1 - 2.4 % |