General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Carbono | 0.55 % Show Material materials with Carbono of 0.55 % |
Cromo | 8 % Show Material materials with Cromo of 8 % |
Hierro | 88.8 - 100 % Show Material materials with Hierro of 88.8 - 100 % |
Manganeso | 0.4 % Show Material materials with Manganeso of 0.4 % |
Molibdeno | 0.75 % Show Material materials with Molibdeno of 0.75 % |
Silicona | 1.5 % Show Material materials with Silicona of 1.5 % |