General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Densidad of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Martensitic Stainless Steel |
Dureza Brinell | 20.0 °C | 266 - 325 [-] Show Material materials with Dureza Brinell of 266 - 325 [-] | |
Elongación A5 | 20.0 °C | 14 - 22 % Show Material materials with Elongación A5 of 14 - 22 % | |
Estricción | 20.0 °C | 40 - 50 % Show Material materials with Estricción of 40 - 50 % | |
Límite elástico | 20.0 °C | 750 MPa Show Material materials with Límite elástico of 750 MPa | |
Módulo elástico | 20.0 °C | 194 - 220 GPa Show Material materials with Módulo elástico of 194 - 220 GPa | Typical for Martensitic Stainless Steel |
Resistencia a la tracción | 20.0 °C | 1100 - 1350 MPa Show Material materials with Resistencia a la tracción of 1100 - 1350 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 - 500 J/(kg·K) Show Material materials with Calor específico of 460 - 500 J/(kg·K) | Typical for Martensitic Stainless Steel |
Coeficiente de dilatación térmica | 100.0 °C | 1.09E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.09E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
200.0 °C | 1.13E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.13E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.15E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.15E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
600.0 °C | 1.24E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.24E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
700.0 °C | 1.18E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.18E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1300.0 °C | 1.35E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.35E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Conductividad térmica | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Conductividad térmica of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Temperatura de fusión | 1375 - 1450 °C Show Material materials with Temperatura de fusión of 1375 - 1450 °C | Typical for Martensitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 20.0 °C | 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.4 - 0.5 % Show Material materials with Carbono of 0.4 - 0.5 % |
Cromo | 8 - 10 % Show Material materials with Cromo of 8 - 10 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 0.8 % Show Material materials with Manganeso of 0.8 % |
Níquel | 0.6 % Show Material materials with Níquel of 0.6 % |
Silicona | 2.7 - 3.3 % Show Material materials with Silicona of 2.7 - 3.3 % |