General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Medium Carbon Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Medium Carbon Steel |
Dureza Rockwell C | 20.0 °C | 35 [-] Show Material materials with Dureza Rockwell C of 35 [-] | |
Elongación A5 | 20.0 °C | 18 % Show Material materials with Elongación A5 of 18 % | |
Estricción | 20.0 °C | 60 % Show Material materials with Estricción of 60 % | |
Límite elástico | 20.0 °C | 960 MPa Show Material materials with Límite elástico of 960 MPa | |
Módulo de cizallamiento | 20.0 °C | 75 - 80 GPa Show Material materials with Módulo de cizallamiento of 75 - 80 GPa | Typical for Carbon Steel |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Medium Carbon Steel |
Resistencia a la tracción | 20.0 °C | 1050 MPa Show Material materials with Resistencia a la tracción of 1050 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 200.0 °C | 1.16E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.16E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
300.0 °C | 1.21E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.21E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.31E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.31E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
600.0 °C | 1.36E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.36E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Conductividad térmica | 20.0 °C | 42 W/(m·K) Show Material materials with Conductividad térmica of 42 W/(m·K) | |
Temperatura de fusión | 1380 - 1514 °C Show Material materials with Temperatura de fusión of 1380 - 1514 °C | Typical for Medium Carbon Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.35 - 0.45 % Show Material materials with Carbono of 0.35 - 0.45 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 1.25 - 1.75 % Show Material materials with Manganeso of 1.25 - 1.75 % |
Silicona | 0.75 % Show Material materials with Silicona of 0.75 % |