General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Límite elástico | 20.0 °C | 520 MPa Show Material materials with Límite elástico of 520 MPa | |
540.0 °C | 110 MPa Show Material materials with Límite elástico of 110 MPa | ||
650.0 °C | 57 MPa Show Material materials with Límite elástico of 57 MPa | ||
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 790 MPa Show Material materials with Resistencia a la tracción of 790 MPa | |
540.0 °C | 140 MPa Show Material materials with Resistencia a la tracción of 140 MPa | ||
650.0 °C | 86 MPa Show Material materials with Resistencia a la tracción of 86 MPa | ||
Chemical properties
Property | Value |
---|---|
Carbono | 0.4 % Show Material materials with Carbono of 0.4 % |
Cromo | 0.65 % Show Material materials with Cromo of 0.65 % |
Hierro | 96.6 - 100 % Show Material materials with Hierro of 96.6 - 100 % |
Manganeso | 0.8 % Show Material materials with Manganeso of 0.8 % |
Níquel | 1.25 % Show Material materials with Níquel of 1.25 % |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |