General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Dureza Rockwell C | 20.0 °C | 35 [-] Show Material materials with Dureza Rockwell C of 35 [-] | |
Elongación A5 | 20.0 °C | 18 % Show Material materials with Elongación A5 of 18 % | |
Estricción | 20.0 °C | 58 % Show Material materials with Estricción of 58 % | |
Límite elástico | 20.0 °C | 1000 MPa Show Material materials with Límite elástico of 1000 MPa | |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Resistencia a la tracción | 20.0 °C | 1100 MPa Show Material materials with Resistencia a la tracción of 1100 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 448 - 502 J/(kg·K) Show Material materials with Calor específico of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | 20.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
200.0 °C | 1.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 1/K | Typical for Chromium Molybdenum Steel | |
300.0 °C | 1.17E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.17E-5 1/K | Typical for Chromium Molybdenum Steel | |
500.0 °C | 1.23E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.23E-5 1/K | Typical for Chromium Molybdenum Steel | |
600.0 °C | 1.26E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.26E-5 1/K | Typical for Chromium Molybdenum Steel | |
Conductividad térmica | 20.0 °C | 36 - 43 W/(m·K) Show Material materials with Conductividad térmica of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.37 - 0.44 % Show Material materials with Carbono of 0.37 - 0.44 % |
Cromo | 0.75 - 1.2 % Show Material materials with Cromo of 0.75 - 1.2 % |
Fósforo | 0.35 % Show Material materials with Fósforo of 0.35 % |
Hierro | Balance |
Manganeso | 0.75 - 1.1 % Show Material materials with Manganeso of 0.75 - 1.1 % |
Molibdeno | 0.15 - 0.25 % Show Material materials with Molibdeno of 0.15 - 0.25 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |