General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Estricción | 23.0 °C | 68 % Show Material materials with Estricción of 68 % | |
Límite elástico | 23.0 °C | 710 MPa Show Material materials with Límite elástico of 710 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 900 MPa Show Material materials with Resistencia a la tracción of 900 MPa |
Chemical properties
Property | Value |
---|---|
Carbono | 0.39 % Show Material materials with Carbono of 0.39 % |
Hierro | 98.61 - 100 % Show Material materials with Hierro of 98.61 - 100 % |
Manganeso | 0.75 % Show Material materials with Manganeso of 0.75 % |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % |