General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Carbono | 2 - 2.5 % Show Material materials with Carbono of 2 - 2.5 % | |
Cromo | 22 - 26 % Show Material materials with Cromo of 22 - 26 % | |
Hierro | 56.25 - 100 % Show Material materials with Hierro of 56.25 - 100 % | Balance |
Molibdeno | 5 - 6 % Show Material materials with Molibdeno of 5 - 6 % | |
Níquel | 10 - 12 % Show Material materials with Níquel of 10 - 12 % | |
Silicona | 0.8 - 1.3 % Show Material materials with Silicona of 0.8 - 1.3 % |