General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 9.7 g/cm³ Show Material materials with Densidad of 9.7 g/cm³ | Typical for Nickel Chromium Cobalt Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 240 GPa Show Material materials with Módulo elástico of 240 GPa | Typical for Nickel Chromium Cobalt Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Calor específico of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Cobalt Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Chromium Cobalt Alloy |
Conductividad térmica | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Conductividad térmica of 8 - 35 W/(m·K) | Typical for Nickel Chromium Cobalt Alloy |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 2 - 2.75 % Show Material materials with Carbono of 2 - 2.75 % |
Cobalto | 9 - 11 % Show Material materials with Cobalto of 9 - 11 % |
Cromo | 27 - 31 % Show Material materials with Cromo of 27 - 31 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 8 % Show Material materials with Hierro of 8 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Silicona | 0.5 - 1 % Show Material materials with Silicona of 0.5 - 1 % |
Wolframio | 14 - 16 % Show Material materials with Wolframio of 14 - 16 % |