General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 9 g/cm³ Show Material materials with Densidad of 9 g/cm³ | Typical for Cobalt Superalloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 6E-7 - 8.7E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 6E-7 - 8.7E-6 1/K | Typical for Cobalt Superalloy |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 1.1 - 1.7 % Show Material materials with Carbono of 1.1 - 1.7 % |
Cromo | 26 - 33 % Show Material materials with Cromo of 26 - 33 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 3 % Show Material materials with Hierro of 3 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 1 % Show Material materials with Molibdeno of 1 % |
Níquel | 3 % Show Material materials with Níquel of 3 % |
Silicona | 0.4 - 2 % Show Material materials with Silicona of 0.4 - 2 % |
Wolframio | 7 - 9.5 % Show Material materials with Wolframio of 7 - 9.5 % |